. Transactions. Brin. d= mm. 1^]^^^ < ^HHH^miiii ^^w ^^^^ i!^ 650° C. ANNEAL Brin. d = mm. Brin. , d= mm. 70u° C. anneal Brin. , d= mm. Fig. 11.—Etched with ammonia and hydrogen peroxide. X 75. W. H. BASSETT AXD C. H. DAVIS 443 PER CENT. REDUCTION PER CENT. REDUCTION