. Corrosion of materials in surface seawater after 12 and 18 months of exposure. Corrosion and anti-corrosives; Alloys. 2 3 4 Oxygen (ml/I) or Corrosion Rate (mpy) Figure 26. Corrosion of 200 and 400 Series stainless steels vs depth after 1 year of exposure. 91. Please note that these images are extracted from scanned page images that may have been digitally enhanced for readability - coloration and appearance of these illustrations may not perfectly resemble the original Reinhart, Frederick Morris, b. 1908; Naval Civil Engineering Laboratory (Port Hueneme, Calif. ); United States. Nava


. Corrosion of materials in surface seawater after 12 and 18 months of exposure. Corrosion and anti-corrosives; Alloys. 2 3 4 Oxygen (ml/I) or Corrosion Rate (mpy) Figure 26. Corrosion of 200 and 400 Series stainless steels vs depth after 1 year of exposure. 91. Please note that these images are extracted from scanned page images that may have been digitally enhanced for readability - coloration and appearance of these illustrations may not perfectly resemble the original Reinhart, Frederick Morris, b. 1908; Naval Civil Engineering Laboratory (Port Hueneme, Calif. ); United States. Naval Facilities Engineering Command. Port Hueneme, Calif. : Naval Civil Engineering Laboratory


Size: 1481px × 1687px
Photo credit: © The Book Worm / Alamy / Afripics
License: Licensed
Model Released: No

Keywords: ., bookcentury1900, booksubj, booksubjectcorrosionandanticorrosives