. Transactions. Fig. 8.—Tantalum wire ax- Fig. 9.—Tantalum wire an- nealed 5 MIN. at 1600° C. IN VACUUM. NEALED 1 MIN. IN HYDROGEN ATMOS- X 125. PHERE. X 125. 632 METALLOGRAPHY OF TUNGSTEN. Fig. 10.—Containing1 PER CENT. Th02. Fig. 11.—Containing2 PER cent. Th02.


Size: 2088px × 1197px
Photo credit: © The Reading Room / Alamy / Afripics
License: Licensed
Model Released: No

Keywords: ., bo, bookcentury1800, bookdecade1870, booksubjectmineralindustries