. Deposition, corrosion and coloration of tungsten trioxide electrochromic thin films. Thin films. 45 y - P (Torr) igure Time needed to bleach the WO films to 50" of the original optical density versus oxygen partial pressure during deposition. (E: V Thickness 3,000 A). Please note that these images are extracted from scanned page images that may have been digitally enhanced for readability - coloration and appearance of these illustrations may not perfectly resemble the original Sun, Sey-Shing.