. Deposition, corrosion and coloration of tungsten trioxide electrochromic thin films. Thin films. T9^. 1000/T (°K ) Figure Temperature dependence of current in W0? films pre- pared at two extreme conditions: solid circles: 'WO, ' and open circles: 'WO Please note that these images are extracted from scanned page images that may have been digitally enhanced for readability - coloration and appearance of these illustrations may not perfectly resemble the original Sun, Sey-Shing.