Archive image from page 51 of Deposition, corrosion and coloration of. Deposition, corrosion and coloration of tungsten trioxide electrochromic thin films depositioncorros00suns Year: 1983 45 y - P (Torr) igure Time needed to bleach the WO films to 50' of the original optical density versus oxygen partial pressure during deposition. (E: V Thickness 3,000 A)